耐諾復(fù)合鋯珠(NanorZr-85):
采用優(yōu)質(zhì)的釔穩(wěn)定的氧化鋯粉和其它氧化物滴定滾動(dòng)成坯,中溫焙燒定相的工藝制成。珠子由均勻的鋁增韌氧化鋯晶粒組成,拒絕了空腔珠、尾巴珠和雪人珠等。優(yōu)異的球形度和中高的密度增加了研磨效率, 超高的耐壓強(qiáng)度可匹配高線速度的砂磨機(jī),是釔穩(wěn)定氧化鋯珠的經(jīng)濟(jì)代替品。
氧化鋯/氧化釔含量: 90%, 氧化鋁含量: 10%,
比 重: >5.2kg/dm3, 散 重: >3.2kg/L,
莫 氏 硬度: 8.5, 耐 壓 強(qiáng)度: 1800N(2mm),
顏 色: 米白, 粒 徑: 0.8-6.0mm,
包 裝: 25kg/桶
NanorZr-85 Alumina Toughen Zirconia(ATZ) beads are shaped by granulated method and sinter in high temperature. The compact and homogenous microstructure say no to the air pocket, the tail and snowman beads. The prfect sphericity and middle to high gravity increase the grinding sfficiency; Maching high quliti contact parts of mills was its disadvantage.
ZrO2/Y2O3 %: 90, Al2O3 %: 10
Density: >5.2kg/dm3, Hardness Vickers: >1150kg/mm2
Crushing Strength: 1800N (2mm), Sizes: 0.6-6.0mm ,
Packing: 25kg/bucket